Slag inclusions casting defect are non-metallic impurities that can form during the melting and pouring of metal. They typically arise from the reaction of molten metal with oxides formed due to more contact time with air during filling of molten metal during die filling. When these oxides formed become entrapped in the solidifying metal, they can lead to various issues, including reduced mechanical properties, compromised surface finish, and, ultimately, product failure.
More chances of slag inclusion occur at low temperatures and more contact time with oxygen that is present in environment and die. More time metal is exposed to oxygen, more slag is formed by converting in molten metal into oxide form.
Various factors contribute to the formation of slag, including
Remedies to avoid slag formation:
Through using casting simulation tools such as ADSTEFAN – Hitachi ICS – Japan based software, Design engineer can access flow conditions of molten metal in cavity whether for given conditions and gating design any turbulence is detected in cavity. This early detection helps design team to remodify gating design and reiterate simulations and best conditions and gating design can be selected and followed by die development and shop floor trails.

a. Air contact results in ADSTEFAN simulation software
Above figure demonstrates air contact time of molten metal inside cavity for gravity die casting process with ADSTEFAN simulation software results. Higher contact time with molten metal and air, higher chances of slag inclusion in casting. Design engineer can also validate temperature distribution and filling velocity of molten metal during filling of mold cavity.
Preventive action taken on component by Gating optimization and process parameter optimization to reduce more contact time with air, high filling velocities and thus slag inclusion defect is controlled. This optimization is carried out in ADSTEFAN software and best gating design, and process parameters are considered in shop floor trails thus leading to elimination of slag inclusion defect in shopfloor. By performing corrective actions using ADSTEFAN casting simulation software, we are able to reduce shop floor trails, production, and development time of component.